前言:PA66日本东丽CM1011G-30高流动尼龙66
CM1011G-30PA6 | 聚已内酰胺#尼龙6日本东丽规格级别: 注塑备注说明: 特性:玻璃30%强化,高流动。CM1011G-30 物性表基本性能额定值单位测试方法吸水率 (23℃.24小时)无水|2.5%水1.1|-%物理性能额定值单位测试方法比重无水|2.5%水1.36|-ASTM D-792机械性能额定值单位测试方法IZOD冲击强度 (无缺口1/8.23℃)无水|2.5%水80|100kg·cm/cm挠曲强度 (80℃)无水|2.5%水1500|1000Kg/cmASTM D-790抗剪强度 (23℃)无水|2.5%水890|700Kg/cmASTM D-732断裂伸长率ASTM D-638 (80℃)无水|2.5%水6|-% (23℃)无水|2.5%水5|5%洛氏硬度ASTM D-785 (23℃)无水|2.5%水120|-R-标度 (23℃)无水|2.5%水93|-M-标度抗拉屈服强度 (80℃)无水|2.5%水1000|700Kg/cmASTM D-638挠曲模量 (-40℃)无水|2.5%水108000|90000Kg/cmASTM D-790挠曲强度 (23℃)无水|2.5%水2600|1400Kg/cmASTM D-790压缩强度ASTM D-695 (-40℃)无水|2.5%水2500|-Kg/cm (80℃)无水|2.5%水970|-Kg/cm挠曲模量 (80℃)无水|2.5%水43000|34000Kg/cmASTM D-790断裂伸长率 (-40℃)无水|2.5%水4.5|-%ASTM D-638挠曲模量 (23℃)无水|2.5%水80000|48000Kg/cmASTM D-790挠曲强度 (-40℃)无水|2.5%水3100|3000Kg/cmASTM D-790抗剪强度 (80℃)无水|2.5%水7000|520Kg/cmASTM D-792压缩强度 (23℃)无水|2.5%水1800|-Kg/cmASTM D-695抗拉屈服强度 (-40℃)无水|2.5%水2550|2300Kg/cmASTM D-638IZOD冲击强度 (V-缺口1/2.-40℃)无水|2.5%水8.5|14kg·cm/cmASTM D-256泰伯磨耗量 ((1000g,CS-17)23℃)无水|2.5%水12|-mg/1000次ASTM D-1044IZOD冲击强度 (无缺口1/8.-40℃)无水|2.5%水68|79kg·cm/cm (V-缺口1/2.23℃)无水|2.5%水11|19kg·cm/cmASTM D-256抗拉屈服强度 (23℃)无水|2.5%水1700|1050Kg/cmASTM D-638电气性能额定值单位测试方法抗电弧性 (1/8")无水|2.5%水131|137秒ASTM D-495介电常数 (50Hz)无水|2.5%水4.9|10.7ASTM D-150体积电阻率无水|2.5%水10|10Ω.cmASTM D-257损耗因数ASTM D-150 (50Hz)无水|2.5%水0.03|0.17 (10Hz)无水|2.5%水0.03|0.18介电常数 (10Hz)无水|2.5%水4.6|7.9ASTM D-150损耗因数 (10Hz)无水|2.5%水0.02|0.07ASTM D-150介电强度 (1/8")无水|2.5%水20|18KV/mmASTM D-149介电常数 (10Hz)无水|2.5%水4.0|4.3ASTM D-150热性能额定值单位测试方法导热系数无水|2.5%水0.23|-Kcal/m·hr·℃熔点无水|2.5%水225|-℃差示扫描测热计DSC线性热膨胀系数无水|2.5%水2-3|-×10-5cm/cm/℃ASTM D-696热挠曲温度 (4.6kg/cm)无水|2.5%水224|-℃ASTM D-648UL-94抗燃级无水|2.5%水|无水|2.5%水UL-94|-|HB(1/16")|-UL 94热挠曲温度 (18.6kg/cm)无水|2.5%水215|-℃ASTM D-648比热无水|2.5%水0.32|-Cal/g·℃其它性能额定值单位测试方法强化含量无水|2.5%水30|-温馨提示:我司产品均可免费提供详细物性表(英文和中文版)、加工参数表、ROHS、、MSDS、UL及FDA等认证相关资料;可免费为客户分析样版并提供原料型号咨询服务(可免费帮客户翻译英文资料);如需试料、了解产品相关信息及当日报价,敬请来电、来邮或在线咨询,我们将竭诚为您服务!郑重承诺:本公司所销售原料全部为原厂原包正牌料、杜绝一切副牌料、水口料以次充好。企业新闻